PropertyL 605Phynox (Co-20Cr-15Ni-7Mo-Fe) annealedDifference
Tensile strength970 MPa770 MPa-21%
Elongation52 %50 %-4%
Elastic modulus225,000 MPa210,000 MPa-7%
Density9,130 kg/m³8,300 kg/m³-9%
Coefficient of thermal expansion0.000012 1/K0.000015 1/K+23%
Melting point1,370 °C1,420 °C+4%

Difference is Phynox (Co-20Cr-15Ni-7Mo-Fe) annealed relative to L 605. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

L 605
grade
R30605
standard
Haynes International datasheet H-3000C
heat treatment
annealed
Phynox (Co-20Cr-15Ni-7Mo-Fe) annealed
grade
R30003
standard
Aperam PHYNOX datasheet 2020 (ASTM F1058)
heat treatment
annealed