Home/Compare/Cobalt Alloy/Hs 188 vs Phynox (Co-20Cr-15Ni-7Mo-Fe) annealed

Hs 188 vs Phynox (Co-20Cr-15Ni-7Mo-Fe) annealed

Property comparison of Hs 188 and Phynox (Co-20Cr-15Ni-7Mo-Fe) annealed, both cobalt alloy.

Cobalt Alloy6 compared properties
PropertyHs 188Phynox (Co-20Cr-15Ni-7Mo-Fe) annealedDifference
Tensile strength946 MPa770 MPa-19%
Elongation53 %50 %-6%
Elastic modulus232,000 MPa210,000 MPa-9%
Density8,980 kg/m³8,300 kg/m³-8%
Coefficient of thermal expansion0.000011 1/K0.000015 1/K+35%
Melting point1,316 °C1,420 °C+8%

Difference is Phynox (Co-20Cr-15Ni-7Mo-Fe) annealed relative to Hs 188. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Hs 188
grade
R30188
standard
Haynes International datasheet H-3125C
heat treatment
annealed (bright)
Phynox (Co-20Cr-15Ni-7Mo-Fe) annealed
grade
R30003
standard
Aperam PHYNOX datasheet 2020 (ASTM F1058)
heat treatment
annealed