PropertyElgiloy (Co-20Cr-15Ni-7Mo-Fe) annealedHs 188Difference
Yield strength310 MPa464 MPa+50%
Elastic modulus193,000 MPa232,000 MPa+20%
Poisson ratio0.30.31+3%
Density8,300 kg/m³8,980 kg/m³+8%
Thermal conductivity12.5 W/m·K10.8 W/m·K-14%
Coefficient of thermal expansion0.000015 1/K0.000011 1/K-26%
Melting point1,420 °C1,316 °C-7%

Difference is Hs 188 relative to Elgiloy (Co-20Cr-15Ni-7Mo-Fe) annealed. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Elgiloy (Co-20Cr-15Ni-7Mo-Fe) annealed
grade
R30003
standard
Elgiloy Specialty Metals Wire Data Sheet (ASTM F1058 / AMS 5833)
heat treatment
annealed
Hs 188
grade
R30188
standard
Haynes International datasheet H-3125C
heat treatment
annealed (bright)