PropertyHigh Leaded Tin Bronze C94500Nickel-Tin Bronze C94800Difference
Yield strength83 MPa159 MPa+92%
Tensile strength172 MPa310 MPa+80%
Elongation12 %35 %+192%
Elastic modulus120,000 MPa120,000 MPa0%
Shear modulus45,000 MPa45,000 MPa0%
Poisson ratio0.310.310%
Density8,800 kg/m³8,800 kg/m³0%
Thermal conductivity50 W/m·K50 W/m·K0%
Specific heat377 J/kg·K377 J/kg·K0%
Coefficient of thermal expansion0.000019 1/K0.000019 1/K0%
Melting point925 °C925 °C0%

Difference is Nickel-Tin Bronze C94800 relative to High Leaded Tin Bronze C94500. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

High Leaded Tin Bronze C94500
standard
ANSI
Nickel-Tin Bronze C94800
standard
ANSI

What else is in Engineering Database

Related comparisons

View each material