Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Copper Alloy/High Leaded Tin Bronze C94300 vs High Leaded Tin Bronze C94500

High Leaded Tin Bronze C94300 vs High Leaded Tin Bronze C94500

Property comparison of High Leaded Tin Bronze C94300 and High Leaded Tin Bronze C94500, both copper alloy.

Copper Alloy11 compared properties
PropertyHigh Leaded Tin Bronze C94300High Leaded Tin Bronze C94500Difference
Yield strength90 MPa83 MPa-8%
Tensile strength186 MPa172 MPa-8%
Elongation15 %12 %-20%
Elastic modulus120,000 MPa120,000 MPa0%
Shear modulus45,000 MPa45,000 MPa0%
Poisson ratio0.310.310%
Density8,800 kg/m³8,800 kg/m³0%
Thermal conductivity50 W/m·K50 W/m·K0%
Specific heat377 J/kg·K377 J/kg·K0%
Coefficient of thermal expansion0.000019 1/K0.000019 1/K0%
Melting point925 °C925 °C0%

Difference is High Leaded Tin Bronze C94500 relative to High Leaded Tin Bronze C94300. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

High Leaded Tin Bronze C94300
standard
ANSI
High Leaded Tin Bronze C94500
standard
ANSI