High Leaded Tin Bronze C94500 vs Nickel-Tin Bronze C94700
Property comparison of High Leaded Tin Bronze C94500 and Nickel-Tin Bronze C94700, both copper alloy.
| Property | High Leaded Tin Bronze C94500 | Nickel-Tin Bronze C94700 | Difference |
|---|---|---|---|
| Yield strength | 83 MPa | 159 MPa | +92% |
| Tensile strength | 172 MPa | 345 MPa | +101% |
| Elongation | 12 % | 35 % | +192% |
| Elastic modulus | 120,000 MPa | 120,000 MPa | 0% |
| Shear modulus | 45,000 MPa | 45,000 MPa | 0% |
| Poisson ratio | 0.31 | 0.31 | 0% |
| Density | 8,800 kg/m³ | 8,800 kg/m³ | 0% |
| Thermal conductivity | 50 W/m·K | 50 W/m·K | 0% |
| Specific heat | 377 J/kg·K | 377 J/kg·K | 0% |
| Coefficient of thermal expansion | 0.000019 1/K | 0.000019 1/K | 0% |
| Melting point | 925 °C | 925 °C | 0% |
Difference is Nickel-Tin Bronze C94700 relative to High Leaded Tin Bronze C94500. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
- standard
- ANSI
- standard
- ANSI
What else is in Engineering Database
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators