Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Nickel Alloy/Hastelloy C-22 vs Hastelloy N

Hastelloy C-22 vs Hastelloy N

Property comparison of Hastelloy C-22 and Hastelloy N, both nickel alloy.

Nickel Alloy6 compared properties
PropertyHastelloy C-22Hastelloy NDifference
Elongation57 %39 %-32%
Elastic modulus206,000 MPa219,000 MPa+6%
Density8,690 kg/m³8,860 kg/m³+2%
Thermal conductivity9.6 W/m·K11.5 W/m·K+20%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K-1%
Melting point1,378 °C1,372 °C0%

Difference is Hastelloy N relative to Hastelloy C-22. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Hastelloy C-22
grade
C-22
standard
Haynes International Datasheet H-2019
heat treatment
Annealed
Hastelloy N
grade
N
standard
Haynes International Datasheet H-3009
heat treatment
Annealed

About Hastelloy nickel-molybdenum superalloys

Hastelloy is a family of nickel-molybdenum-chromium alloys built for severe corrosion service. C-276 is the workhorse for chemical process equipment and handles wet chlorine, hypochlorite, and ferric chloride. B-series grades focus on hydrochloric acid resistance.