Property comparison of Hastelloy C-22 and Hastelloy C-276, both nickel alloy.

Nickel Alloy10 compared properties
PropertyHastelloy C-22Hastelloy C-276Difference
Yield strength403 MPa360 MPa-11%
Tensile strength802 MPa790 MPa-1%
Elongation57 %58 %+2%
Elastic modulus206,000 MPa205,000 MPa0%
Poisson ratio0.310.310%
Density8,690 kg/m³8,890 kg/m³+2%
Thermal conductivity9.6 W/m·K10.2 W/m·K+6%
Specific heat410 J/kg·K427 J/kg·K+4%
Coefficient of thermal expansion0.000012 1/K0.000013 1/K+2%
Melting point1,378 °C1,347 °C-2%

Difference is Hastelloy C-276 relative to Hastelloy C-22. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Hastelloy C-22
grade
C-22
standard
Haynes International Datasheet H-2019
heat treatment
Annealed
Hastelloy C-276
grade
C-276
standard
Haynes International Datasheet H-2002
heat treatment
Annealed

About Hastelloy nickel-molybdenum superalloys