Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Nickel Alloy/Hastelloy C-22 vs Hastelloy G-35

Hastelloy C-22 vs Hastelloy G-35

Property comparison of Hastelloy C-22 and Hastelloy G-35, both nickel alloy.

Nickel Alloy10 compared properties
PropertyHastelloy C-22Hastelloy G-35Difference
Yield strength403 MPa345 MPa-14%
Tensile strength802 MPa738 MPa-8%
Elongation57 %60 %+5%
Elastic modulus206,000 MPa204,000 MPa-1%
Poisson ratio0.310.3-3%
Density8,690 kg/m³8,220 kg/m³-5%
Thermal conductivity9.6 W/m·K10 W/m·K+4%
Specific heat410 J/kg·K450 J/kg·K+10%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K-1%
Melting point1,378 °C1,347 °C-2%

Difference is Hastelloy G-35 relative to Hastelloy C-22. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Hastelloy C-22
grade
C-22
standard
Haynes International Datasheet H-2019
heat treatment
Annealed
Hastelloy G-35
grade
G-35
standard
Haynes International Datasheet H-3084
heat treatment
Annealed

About Hastelloy nickel-molybdenum superalloys

Hastelloy is a family of nickel-molybdenum-chromium alloys built for severe corrosion service. C-276 is the workhorse for chemical process equipment and handles wet chlorine, hypochlorite, and ferric chloride. B-series grades focus on hydrochloric acid resistance.