Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Carbon Steel/EN C45 vs EN C50

EN C45 vs EN C50

Property comparison of EN C45 and EN C50, both carbon steel.

Carbon Steel11 compared properties
PropertyEN C45EN C50Difference
Yield strength430 MPa460 MPa+7%
Tensile strength650 MPa700 MPa+8%
Elongation16 %15 %-6%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity55.9 W/m·K54 W/m·K-3%
Specific heat464 J/kg·K465 J/kg·K0%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is EN C50 relative to EN C45. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

EN C45
standard
ISO
heat treatment
heat treated
EN C50
standard
ISO
heat treatment
heat treated