Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Carbon Steel/EN C40 vs EN C45

EN C40 vs EN C45

Property comparison of EN C40 and EN C45, both carbon steel.

Carbon Steel11 compared properties
PropertyEN C40EN C45Difference
Yield strength400 MPa430 MPa+8%
Tensile strength630 MPa650 MPa+3%
Elongation18 %16 %-11%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity57.8 W/m·K55.9 W/m·K-3%
Specific heat462 J/kg·K464 J/kg·K0%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is EN C45 relative to EN C40. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

EN C40
standard
ISO
heat treatment
EN C45
standard
ISO
heat treatment
heat treated

What else is in Engineering Database

Related comparisons

View each material