EN C35 vs EN C50

Property comparison of EN C35 and EN C50, both carbon steel.

Carbon Steel11 compared properties
PropertyEN C35EN C50Difference
Yield strength380 MPa460 MPa+21%
Tensile strength600 MPa700 MPa+17%
Elongation16 %15 %-6%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity59.7 W/m·K54 W/m·K-10%
Specific heat461 J/kg·K465 J/kg·K+1%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is EN C50 relative to EN C35. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

EN C35
standard
ISO
heat treatment
EN C50
standard
ISO
heat treatment
heat treated

What else is in Engineering Database

Related comparisons

View each material