Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Carbon Steel/EN 20MnCr5 vs EN 28Mn6

EN 20MnCr5 vs EN 28Mn6

Property comparison of EN 20MnCr5 and EN 28Mn6, both carbon steel.

Carbon Steel11 compared properties
PropertyEN 20MnCr5EN 28Mn6Difference
Yield strength680 MPa490 MPa-28%
Tensile strength980 MPa700 MPa-29%
Elongation8 %15 %+88%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity65.4 W/m·K62.4 W/m·K-5%
Specific heat457 J/kg·K459 J/kg·K0%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is EN 28Mn6 relative to EN 20MnCr5. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

EN 20MnCr5
standard
ISO
heat treatment
case-hardened
EN 28Mn6
standard
ISO
heat treatment
heat treated