PropertyEN 16Mo3EN 28Mn6Difference
Yield strength270 MPa490 MPa+81%
Tensile strength440 MPa700 MPa+59%
Elongation24 %15 %-38%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity66.9 W/m·K62.4 W/m·K-7%
Specific heat456 J/kg·K459 J/kg·K+1%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is EN 28Mn6 relative to EN 16Mo3. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

EN 16Mo3
standard
ISO
heat treatment
EN 28Mn6
standard
ISO
heat treatment
heat treated

What else is in Engineering Database

Related comparisons

View each material