PropertyEN 17Cr3EN 20MnCr5Difference
Yield strength340 MPa680 MPa+100%
Tensile strength580 MPa980 MPa+69%
Elongation14 %8 %-43%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity51.9 W/m·K65.4 W/m·K+26%
Specific heat456 J/kg·K457 J/kg·K0%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is EN 20MnCr5 relative to EN 17Cr3. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

EN 17Cr3
standard
ISO
heat treatment
EN 20MnCr5
standard
ISO
heat treatment
case-hardened

What else is in Engineering Database

Related comparisons

View each material