ATI 75 (UNS N06075) vs ATI 901
Property comparison of ATI 75 (UNS N06075) and ATI 901, both nickel alloy.
| Property | ATI 75 (UNS N06075) | ATI 901 | Difference |
|---|---|---|---|
| Yield strength | 448 MPa | 1,172 MPa | +162% |
| Tensile strength | 813 MPa | 1,276 MPa | +57% |
| Elongation | 32 % | 25 % | -22% |
| Density | 8,370 kg/m³ | 8,220 kg/m³ | -2% |
Difference is ATI 901 relative to ATI 75 (UNS N06075). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
ATI 75 (UNS N06075)
- grade
- N06075
- standard
- ATI Technical Data Sheet
- heat treatment
- Solution Annealed
ATI 901
- grade
- Ni-Fe-Cr-Mo-Ti (N09901)
- standard
- UNS N09901
- heat treatment
- Aged (bar)
What else is in Engineering Database
Iron Engine ↗Engineering AI at ironengine.ai
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculatorsRelated comparisons
ATI 601 (UNS N06601)vsATI 75 (UNS N06075)ATI 601 (UNS N06601)vsATI 901ATI 6230 (UNS N06230)vsATI 75 (UNS N06075)ATI 6230 (UNS N06230)vsATI 901ATI 690vsATI 75 (UNS N06075)ATI 690vsATI 901ATI 718Plus (UNS N07818) Solution Treated and AgedvsATI 75 (UNS N06075)ATI 718Plus (UNS N07818) Solution Treated and AgedvsATI 901