PropertyATI 718Plus (UNS N07818) Solution Treated and AgedATI 901Difference
Yield strength1,145 MPa1,172 MPa+2%
Tensile strength1,476 MPa1,276 MPa-14%
Elongation28 %25 %-11%
Density8,250 kg/m³8,220 kg/m³0%

Difference is ATI 901 relative to ATI 718Plus (UNS N07818) Solution Treated and Aged. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

ATI 718Plus (UNS N07818) Solution Treated and Aged
grade
N07818
standard
ATI Technical Data Sheet
heat treatment
Solution Treated and Aged 788C/704C
ATI 901
grade
Ni-Fe-Cr-Mo-Ti (N09901)
standard
UNS N09901
heat treatment
Aged (bar)