Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Nickel Alloy/ATI 718Plus (UNS N07818) Solution Treated and Aged vs ATI 75 (UNS N06075)

ATI 718Plus (UNS N07818) Solution Treated and Aged vs ATI 75 (UNS N06075)

Property comparison of ATI 718Plus (UNS N07818) Solution Treated and Aged and ATI 75 (UNS N06075), both nickel alloy.

Nickel Alloy5 compared properties
PropertyATI 718Plus (UNS N07818) Solution Treated and AgedATI 75 (UNS N06075)Difference
Yield strength1,145 MPa448 MPa-61%
Tensile strength1,476 MPa813 MPa-45%
Elongation28 %32 %+14%
Density8,250 kg/m³8,370 kg/m³+1%
Melting point1,302 °C1,360 °C+4%

Difference is ATI 75 (UNS N06075) relative to ATI 718Plus (UNS N07818) Solution Treated and Aged. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

ATI 718Plus (UNS N07818) Solution Treated and Aged
grade
N07818
standard
ATI Technical Data Sheet
heat treatment
Solution Treated and Aged 788C/704C
ATI 75 (UNS N06075)
grade
N06075
standard
ATI Technical Data Sheet
heat treatment
Solution Annealed