Stainless Steel8 compared properties
PropertyATI 409HP Ferritic Stainless SteelATI 410S Ferritic Stainless Steel (ASTM Minimum)Difference
Yield strength241 MPa290 MPa+20%
Tensile strength434 MPa444 MPa+2%
Elongation33 %33 %0%
Elastic modulus200,000 MPa200,000 MPa0%
Density7,760 kg/m³7,730 kg/m³0%
Thermal conductivity25 W/m·K26.9 W/m·K+8%
Specific heat477 J/kg·K460 J/kg·K-4%
Coefficient of thermal expansion0.000011 1/K0.000011 1/K+3%

Difference is ATI 410S Ferritic Stainless Steel (ASTM Minimum) relative to ATI 409HP Ferritic Stainless Steel. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

ATI 409HP Ferritic Stainless Steel
grade
UNS S40900/S40930
standard
ASTM A240/A240M
heat treatment
Annealed
ATI 410S Ferritic Stainless Steel (ASTM Minimum)
grade
UNS S41008
standard
ASTM A240
heat treatment
Annealed

About ferritic stainless steels

Ferritic stainless steels are magnetic, body-centered cubic, and cannot be hardened by heat treatment. They are cheaper than austenitic grades because they carry little or no nickel. 409 and 439 are the standard automotive exhaust grades; 444 and the superferritic grades (29-4C, E-Brite) handle chloride and seawater service better than 316 at lower nickel cost.