Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Stainless Steel/ATI 409Cb Ferritic Stainless Steel vs ATI 409HP Ferritic Stainless Steel

ATI 409Cb Ferritic Stainless Steel vs ATI 409HP Ferritic Stainless Steel

Property comparison of ATI 409Cb Ferritic Stainless Steel and ATI 409HP Ferritic Stainless Steel, both stainless steel.

Stainless Steel8 compared properties
PropertyATI 409Cb Ferritic Stainless SteelATI 409HP Ferritic Stainless SteelDifference
Yield strength241 MPa241 MPa0%
Tensile strength434 MPa434 MPa0%
Elongation33 %33 %0%
Elastic modulus200,000 MPa200,000 MPa0%
Density7,760 kg/m³7,760 kg/m³0%
Thermal conductivity25 W/m·K25 W/m·K0%
Specific heat477 J/kg·K477 J/kg·K0%
Coefficient of thermal expansion0.000011 1/K0.000011 1/K0%

Difference is ATI 409HP Ferritic Stainless Steel relative to ATI 409Cb Ferritic Stainless Steel. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

ATI 409Cb Ferritic Stainless Steel
grade
UNS S40945
standard
ASTM A240/A240M
heat treatment
Annealed
ATI 409HP Ferritic Stainless Steel
grade
UNS S40900/S40930
standard
ASTM A240/A240M
heat treatment
Annealed

About ferritic stainless steels

Ferritic stainless steels are magnetic, body-centered cubic, and cannot be hardened by heat treatment. They are cheaper than austenitic grades because they carry little or no nickel. 409 and 439 are the standard automotive exhaust grades; 444 and the superferritic grades (29-4C, E-Brite) handle chloride and seawater service better than 316 at lower nickel cost.