Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Stainless Steel/ATI 201LN Austenitic Stainless Steel (Cryogenic Grade) vs ATI 302 Austenitic Stainless Steel

ATI 201LN Austenitic Stainless Steel (Cryogenic Grade) vs ATI 302 Austenitic Stainless Steel

Property comparison of ATI 201LN Austenitic Stainless Steel (Cryogenic Grade) and ATI 302 Austenitic Stainless Steel, both stainless steel.

Stainless Steel5 compared properties
PropertyATI 201LN Austenitic Stainless Steel (Cryogenic Grade)ATI 302 Austenitic Stainless SteelDifference
Yield strength320 MPa205 MPa-36%
Tensile strength685 MPa515 MPa-25%
Elongation51 %40 %-22%
Elastic modulus193,000 MPa200,000 MPa+4%
Density7,840 kg/m³7,900 kg/m³+1%

Difference is ATI 302 Austenitic Stainless Steel relative to ATI 201LN Austenitic Stainless Steel (Cryogenic Grade). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

ATI 201LN Austenitic Stainless Steel (Cryogenic Grade)
grade
201LN
standard
ASTM A240; ASME SA-240; ASTM A666
heat treatment
Mill Annealed
ATI 302 Austenitic Stainless Steel
grade
302
standard
ASTM A240
heat treatment
Annealed

About austenitic stainless steels

Austenitic stainless steels are the largest stainless family. They are non-magnetic in the annealed condition and gain corrosion resistance from chromium and nickel (and molybdenum in 316-class grades). They cannot be hardened by heat treatment and rely on cold work for higher strength. Includes the 300-series, super-austenitic grades (904L, AL-6XN), and high-nitrogen variants used in pressure vessels and chemical service.

What else is in Engineering Database

Related comparisons

View each material