Stainless Steel5 compared properties
PropertyATI 201 HP Austenitic Stainless SteelATI 201LN Austenitic Stainless Steel (Cryogenic Grade)Difference
Yield strength301 MPa320 MPa+6%
Tensile strength696 MPa685 MPa-2%
Elongation56 %51 %-9%
Elastic modulus207,000 MPa193,000 MPa-7%
Density7,860 kg/m³7,840 kg/m³0%

Difference is ATI 201LN Austenitic Stainless Steel (Cryogenic Grade) relative to ATI 201 HP Austenitic Stainless Steel. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

ATI 201 HP Austenitic Stainless Steel
grade
201 HP
standard
ASTM A240
heat treatment
Annealed
ATI 201LN Austenitic Stainless Steel (Cryogenic Grade)
grade
201LN
standard
ASTM A240; ASME SA-240; ASTM A666
heat treatment
Mill Annealed

About austenitic stainless steels

Austenitic stainless steels are the largest stainless family. They are non-magnetic in the annealed condition and gain corrosion resistance from chromium and nickel (and molybdenum in 316-class grades). They cannot be hardened by heat treatment and rely on cold work for higher strength. Includes the 300-series, super-austenitic grades (904L, AL-6XN), and high-nitrogen variants used in pressure vessels and chemical service.

What else is in Engineering Database

Related comparisons

View each material