Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Stainless Steel/ATI 20 (Superaustenitic) vs ATI 302 Austenitic Stainless Steel

ATI 20 (Superaustenitic) vs ATI 302 Austenitic Stainless Steel

Property comparison of ATI 20 (Superaustenitic) and ATI 302 Austenitic Stainless Steel, both stainless steel.

Stainless Steel8 compared properties
PropertyATI 20 (Superaustenitic)ATI 302 Austenitic Stainless SteelDifference
Yield strength355 MPa205 MPa-42%
Tensile strength641 MPa515 MPa-20%
Elongation38 %40 %+5%
Elastic modulus193,000 MPa200,000 MPa+4%
Density8,080 kg/m³7,900 kg/m³-2%
Thermal conductivity12.2 W/m·K16.3 W/m·K+34%
Specific heat460 J/kg·K460 J/kg·K0%
Coefficient of thermal expansion0.000015 1/K0.000017 1/K+13%

Difference is ATI 302 Austenitic Stainless Steel relative to ATI 20 (Superaustenitic). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

ATI 20 (Superaustenitic)
grade
UNS N08020
standard
ASTM B463
heat treatment
Annealed
ATI 302 Austenitic Stainless Steel
grade
302
standard
ASTM A240
heat treatment
Annealed

About austenitic stainless steels

Austenitic stainless steels are the largest stainless family. They are non-magnetic in the annealed condition and gain corrosion resistance from chromium and nickel (and molybdenum in 316-class grades). They cannot be hardened by heat treatment and rely on cold work for higher strength. Includes the 300-series, super-austenitic grades (904L, AL-6XN), and high-nitrogen variants used in pressure vessels and chemical service.

What else is in Engineering Database

Related comparisons