Property comparison of 17 4PH and 17 7PH, both stainless steel.

Stainless Steel7 compared properties
Property17 4PH17 7PHDifference
Yield strength1,000 MPa1,586 MPa+59%
Tensile strength1,070 MPa1,655 MPa+55%
Elongation12 %1 %-92%
Elastic modulus196,000 MPa200,000 MPa+2%
Density7,750 kg/m³7,810 kg/m³+1%
Brinell hardness331 HB477 HB+44%
Thermal conductivity17.9 W/m·K16 W/m·K-11%

Difference is 17 7PH relative to 17 4PH. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

17 4PH
grade
S17400
standard
AMS 5643 / ASTM A564
heat treatment
H1025
17 7PH
grade
S17700
standard
AMS 5529
heat treatment
CH900

About precipitation-hardening stainless steels

PH grades reach high strength through aging at intermediate temperatures while keeping the corrosion resistance of austenitic or martensitic grades. 17-4 PH and 15-5 PH are the common bar and forging stocks for aerospace and pump shafts. Mechanical properties depend strongly on the aging condition (H900, H1025, H1150).