Stainless Steel6 compared properties
Property17 7PHATI 15-7 PH (Semi-Austenitic)Difference
Yield strength1,586 MPa1,515 MPa-4%
Tensile strength1,655 MPa1,690 MPa+2%
Elongation1 %6 %+500%
Elastic modulus200,000 MPa195,000 MPa-3%
Density7,810 kg/m³7,670 kg/m³-2%
Thermal conductivity16 W/m·K15.1 W/m·K-6%

Difference is ATI 15-7 PH (Semi-Austenitic) relative to 17 7PH. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

17 7PH
grade
S17700
standard
AMS 5529
heat treatment
CH900
ATI 15-7 PH (Semi-Austenitic)
grade
UNS S15700
standard
AMS 5520
heat treatment
Condition RH 950 (1750°F AC / -100°F hold / 950°F age)

About precipitation-hardening stainless steels

PH grades reach high strength through aging at intermediate temperatures while keeping the corrosion resistance of austenitic or martensitic grades. 17-4 PH and 15-5 PH are the common bar and forging stocks for aerospace and pump shafts. Mechanical properties depend strongly on the aging condition (H900, H1025, H1150).