| module category | operating point | ZT | material | notes |
|---|---|---|---|---|
| material_properties_Skutterudite600 | material | 0.88 | Skutterudite | Filled skutterudite at 600C (873K): ZT~0.88, near peak performance. zTavg n-SKD=0.88, p-SKD=0.72 per OSTI 2024 segmented study. Upper temperature limit ~680C before sublimation/oxidation risk. |
This is a sample. Search the full thermoelectric module performance dataset and 300+ more by creating a free account and accessing the database.
Get started for FREERelated data
high_temp_BiTe3 rowsmaterial_properties_BiTe1001 rowmaterial_properties_BiTe1501 rowmaterial_properties_BiTe2001 rowmaterial_properties_BiTe251 rowmaterial_properties_BiTe501 rowmaterial_properties_HalfHeusler7001 rowmaterial_properties_HalfHeusler9001 rowmaterial_properties_PbTe4001 rowmaterial_properties_PbTe5001 rowmaterial_properties_PbTe6001 rowmaterial_properties_SiGe10001 row