Thermoelectric Module Performance: material_properties_HalfHeusler700
Thermoelectric module (TEC/TEG) performance — Peltier cooler COP, cooling capacity, and voltage at various delta-T and hot-side temperatures, plus thermoelectric material properties (ZT, Seebeck coefficient)
| module category | operating point | ZT | material | notes |
|---|---|---|---|---|
| material_properties_HalfHeusler700 | material | 0.7 | Half-Heusler | Half-Heusler (HH) alloys (e.g., NiTiSn n-type, CoTiSb p-type) at 700C (973K): ZT~0.70. Seebeck ~|200| uV/K; thermal conductivity ~3.5 W/(m-K). Excellent mechanical properties and chemical stability vs SiGe. Emerging for industrial waste heat recovery 500-900C. |
This is a sample. Search the full thermoelectric module performance dataset and 300+ more by creating a free account and accessing the database.
Get started for FREERelated data
high_temp_BiTe3 rowsmaterial_properties_BiTe1001 rowmaterial_properties_BiTe1501 rowmaterial_properties_BiTe2001 rowmaterial_properties_BiTe251 rowmaterial_properties_BiTe501 rowmaterial_properties_HalfHeusler9001 rowmaterial_properties_PbTe4001 rowmaterial_properties_PbTe5001 rowmaterial_properties_PbTe6001 rowmaterial_properties_SiGe10001 rowmaterial_properties_SiGe8001 row