Sgp-Interlayer-12.76 — Laminated Annealed

Glass Type
Laminated Annealed
Shgc (dimensionless)
0.87
Allowable Stress MPa Long (MPa)
7
Allowable Stress MPa Short (MPa)
13
Breakage Pattern
Held in Place
Characteristic Strength MPa (MPa)
36
Deflection Limit L Over (dimensionless)
60
Density Kg per M3 (kg/m^3)
2,500
Modulus of Elasticity GPa (GPa)
71.7
Poisson Ratio (dimensionless)
0.22
Record Key
Sgp INTERLAYER#12.76
Standard
ASTM E1300-16 / Haldimann 2008
Subtype
Sgp Interlayer
Surface Compressive Stress MPa Max (MPa)
0
Surface Compressive Stress MPa Min (MPa)
0
Thermal Conductivity W per mK (W/(m*K))
1
Thermal Expansion Coeff per C (1/degC)
0.000009
Thickness MM (mm)
12.76
Visible Transmittance (dimensionless)
0.87

Source: ASTM E1300-16 / Haldimann 2008

laminated_annealed — record key SGP_interlayer#12.76 · thickness mm 12.76 mm · standard ASTM E1300-16 / Haldimann 2008 · subtype SGP_interlayer · SHGC 0.87 dimensionless | Structural Glass Properties | Engineering Database