Explore the Engineering Database more efficiently by signing up for free. Sign up free
Ti-7Al-4Mo-Annealed — Titanium Alloy
- Category
- Titanium Alloy
- Material Id
- Ti-7Al-4Mo Annealed
- Cte per K (1/K)
- 0.00001
- Density Kg M3 (kg/m3)
- 4,480
- Elastic Modulus MPa (MPa)
- 111,000
- Elongation Percent (%)
- 10
- Grade
- Ti-7Al-4Mo
- Heat Treatment
- Annealed
- Melting Point C (°C)
- 1,005
- Name
- Ti-7Al-4Mo (TIMETAL 7-4) Annealed
- Property Basis
- Typical
- Reduction Percent (%)
- 10
- Specific Heat J kgK (J/(kg·K))
- 515
- Standard
- AMS 4919 / MIL-T-9047
- Tensile Strength MPa (MPa)
- 896
- Test Direction
- Longitudinal
- Thermal Conductivity W mK (W/(m·K))
- 6.1
- Yield Strength MPa (MPa)
- 827
Source: AMS 4919 / Mil-T-9047