Ti-4Al-4Mo-2Sn-Sta — Titanium Alloy

Category
Titanium Alloy
Material Id
Ti-4Al-4Mo-2Sn Sta
Cte per K (1/K)
0.000009
Density Kg M3 (kg/m3)
4,600
Elastic Modulus MPa (MPa)
115,000
Elongation Percent (%)
7
Grade
Ti-4Al-4Mo-2Sn-0.5Si
Heat Treatment
Solution Treated and Aged
Melting Point C (°C)
975
Name
Ti-4Al-4Mo-2Sn-0.5Si (TIMETAL 550) Solution Treated and Aged
Property Basis
Typical
Standard
Bs TA45 / Bs TA47
Tensile Strength MPa (MPa)
1,340
Test Direction
Longitudinal
Thermal Conductivity W mK (W/(m·K))
7.52
Yield Strength MPa (MPa)
1,130

Source: BS TA45 / BS TA47

titanium_alloy — material id Ti-4Al-4Mo-2Sn_STA · name Ti-4Al-4Mo-2Sn-0.5Si (TIMETAL 550) Solution Treated and Aged · tensile strength MPa 1340 MPa · yield strength MPa 1130 MPa · grade Ti-4Al-4Mo-2Sn-0.5Si | Metal Alloy Properties | Engineering Database