Explore the Engineering Database more efficiently by signing up for free. Sign up free
Ti-3.9V-0.85Al-0.25Si-Sta-Wq — Titanium Alloy
- Category
- Titanium Alloy
- Material Id
- Ti-3.9V-0.85Al-0.25Si Sta Wq
- Density Kg M3 (kg/m3)
- 4,530
- Elongation Percent (%)
- 23
- Grade
- Ti-3.9V-0.85Al-0.25Si-0.25Fe
- Heat Treatment
- Solution Treated and Aged (Water Quench)
- Melting Point C (°C)
- 890
- Name
- Ti-3.9V-0.85Al-0.25Si-0.25Fe (TIMETAL 407) Sta Water Quench
- Property Basis
- Typical
- Reduction Percent (%)
- 59
- Specific Heat J kgK (J/(kg·K))
- 533
- Standard
- Timet Proprietary
- Tensile Strength MPa (MPa)
- 882
- Test Direction
- Longitudinal
- Thermal Conductivity W mK (W/(m·K))
- 11.3
- Yield Strength MPa (MPa)
- 776
Source: TIMET Proprietary