Sample data from Engineering Database — 375 reference tables, deterministic calculators, and Engineering AI. Sign up free

Metal Alloy Properties: refractory

Zircadyne 705 Annealed 371C to Zircadyne 705 Annealed 93C

Metal and alloy mechanical properties — tensile/yield strength, elastic modulus, density, hardness for steels, aluminum alloys, copper alloys, titanium, nickel alloys, cast iron, and more

Civil Engineeringcategory: refractory2 rowsPage 4 of 4
categorymaterial idcte per K (1/K)density kg m3 (kg/m3)elastic modulus MPa (MPa)elongation percent (%)gradeheat treatmentmelting point C (°C)namepoisson ratio (dimensionless)property basisshear modulus MPa (MPa)specific heat J kgK (J/(kg·K))standardtensile strength MPa (MPa)test temperature C (C)thermal conductivity W mK (W/(m·K))yield strength MPa (MPa)
refractoryZircadyne 705 Annealed 371C0.0000066,64077,80027.8R60705Annealed1,840Zircadyne 705 (UNS R60705)0.33Typical34,500280.5ASTM B551 / B523 / B493 / B550 / B65828137117.1173
refractoryZircadyne 705 Annealed 93C0.0000046,64093,80030.5R60705Annealed1,840Zircadyne 705 (UNS R60705)0.33Typical34,500280.5ASTM B551 / B523 / B493 / B550 / B658494.79317.1390.7