| category | material id | cte per K (1/K) | density kg m3 (kg/m3) | elastic modulus MPa (MPa) | elongation percent (%) | grade | heat treatment | melting point C (°C) | name | poisson ratio (dimensionless) | property basis | shear modulus MPa (MPa) | specification | standard | tensile strength MPa (MPa) | test direction | thermal conductivity W mK (W/(m·K)) | yield strength MPa (MPa) |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| cobalt_alloy | Elgiloy_Annealed | 0.000015 | 8,300 | 193,000 | — | R30003 | annealed | 1,420 | Elgiloy (Co-20Cr-15Ni-7Mo-Fe) annealed | 0.3 | — | — | — | Elgiloy Specialty Metals Wire Data Sheet (ASTM F1058 / AMS 5833) | — | — | 12.5 | 310 |
| cobalt_alloy | Elgiloy_Full_Hard | 0.000015 | 8,300 | 200,000 | — | R30003 | cold-reduced (full hard) | 1,420 | Elgiloy (Co-20Cr-15Ni-7Mo-Fe) full hard | 0.3 | — | — | — | Elgiloy Specialty Metals Wire Data Sheet (ASTM F1058 / AMS 5833) | 1,930 | — | 12.5 | 1,660 |
| cobalt_alloy | HS_188_SHEET_ST | — | 8,968.2876 | 231,672 | 40 | HS 188 | Solution Treated | — | HS 188 (Haynes 188), Sheet, Solution Treated | 0.31 | S-basis | 88,256 | AMS 5608 | MIL-HDBK-5J | 861.875 | Longitudinal | — | 393.015 |