Mar-M-247-Cast-Heat-Treated — Nickel Alloy

Category
Nickel Alloy
Material Id
Mar-M 247 Cast Heat Treated
Cte per K (1/K)
0.000013
Density Kg M3 (kg/m3)
7,800
Elongation Percent (%)
5
Grade
N/A
Heat Treatment
Investment Cast + Standard Heat Treat
Melting Point C (°C)
1,366
Name
Mar-M 247 (Ni-8.3Cr-10Co-10W-5.5Al-3Ta-1Ti-0.7Mo) Cast Heat Treated
Standard
AZoM Super Alloy Mar-M 247 (ArticleID 7808); Tms Superalloys 1984 Kaufman Et al. Mar-M-247 Turbine Blisk
Tensile Strength MPa (MPa)
1,035
Thermal Conductivity W mK (W/(m·K))
11.3
Yield Strength MPa (MPa)
930

Source: AZoM Super Alloy MAR-M 247 (ArticleID 7808); TMS Superalloys 1984 Kaufman et al. MAR-M-247 turbine blisk