Explore the Engineering Database more efficiently by signing up for free. Sign up free
Ati-22-Annealed — Nickel Alloy
- Category
- Nickel Alloy
- Material Id
- Ati 22 Annealed
- Brinell Hardness (HB)
- 172
- Cte per K (1/K)
- 0.000012
- Density Kg M3 (kg/m3)
- 8,690
- Elastic Modulus MPa (MPa)
- 207,000
- Elongation Percent (%)
- 67
- Grade
- N06022
- Heat Treatment
- Annealed
- Melting Point C (°C)
- 1,371
- Name
- Ati 22 (UNS N06022)
- Property Basis
- Typical
- Specific Heat J kgK (J/(kg·K))
- 422
- Standard
- Ati Technical Data Sheet
- Tensile Strength MPa (MPa)
- 724
- Thermal Conductivity W mK (W/(m·K))
- 9.4
- Yield Strength MPa (MPa)
- 345
Source: ATI Technical Data Sheet