Haynes-282-Aged — Nickel Alloy

Category
Nickel Alloy
Material Id
Haynes 282 Aged
Cte per K (1/K)
0.000012
Density Kg M3 (kg/m3)
8,290
Elastic Modulus MPa (MPa)
217,000
Electrical Resistivity uOhm M (uOhm*m)
1.261
Elongation Percent (%)
33
Grade
282
Heat Treatment
Aged (Solution Annealed + Double Aged)
Melting Point C (°C)
1,338
Name
Haynes 282
Poisson Ratio (dimensionless)
0.3
Specific Heat J kgK (J/(kg·K))
436
Standard
Haynes International Datasheet H-3173
Tensile Strength MPa (MPa)
1,132
Thermal Conductivity W mK (W/(m·K))
10.3
Yield Strength MPa (MPa)
699

Source: Haynes International Datasheet H-3173