Explore the Engineering Database more efficiently by signing up for free. Sign up free

Haynes-214-Annealed — Nickel Alloy

Category
Nickel Alloy
Material Id
Haynes 214 Annealed
Cte per K (1/K)
0.000013
Density Kg M3 (kg/m3)
8,050
Elastic Modulus MPa (MPa)
218,000
Electrical Resistivity uOhm M (uOhm*m)
1.359
Elongation Percent (%)
37.3
Grade
214
Heat Treatment
Annealed
Melting Point C (°C)
1,378
Name
Haynes 214
Poisson Ratio (dimensionless)
0.3
Standard
Haynes International Datasheet H-3008
Tensile Strength MPa (MPa)
975
Thermal Conductivity W mK (W/(m·K))
12
Yield Strength MPa (MPa)
577

Source: Haynes International Datasheet H-3008

nickel_alloy — material id Haynes_214_Annealed · name Haynes 214 · grade 214 · tensile strength MPa 975 MPa · yield strength MPa 577 MPa | Metal Alloy Properties | Engineering Database