Hastelloy-C-22-Annealed — Nickel Alloy

Category
Nickel Alloy
Material Id
Hastelloy C-22 Annealed
Cte per K (1/K)
0.000012
Density Kg M3 (kg/m3)
8,690
Elastic Modulus MPa (MPa)
206,000
Electrical Resistivity uOhm M (uOhm*m)
1.14
Elongation Percent (%)
57
Grade
C-22
Heat Treatment
Annealed
Melting Point C (°C)
1,378
Name
Hastelloy C-22
Poisson Ratio (dimensionless)
0.31
Specific Heat J kgK (J/(kg·K))
410
Standard
Haynes International Datasheet H-2019
Tensile Strength MPa (MPa)
802
Thermal Conductivity W mK (W/(m·K))
9.6
Yield Strength MPa (MPa)
403

Source: Haynes International Datasheet H-2019