Lead-Tellurium-PbTe — Lead Alloy

Category
Lead Alloy
Material Id
Lead Tellurium PbTe
Brinell Hardness (HB)
5
Cte per K (1/K)
0.000029
Density Kg M3 (kg/m3)
11,340
Elastic Modulus MPa (MPa)
16,000
Elongation Percent (%)
40
Grade
Tellurium Lead
Heat Treatment
Wrought
Melting Point C (°C)
327
Name
Lead-Tellurium (Pb-0.04Te)
Specific Heat J kgK (J/(kg·K))
128
Standard
Asm Handbook Vol. 2
Tensile Strength MPa (MPa)
22
Thermal Conductivity W mK (W/(m·K))
35
Yield Strength MPa (MPa)
12

Source: ASM Handbook Vol. 2