Explore the Engineering Database more efficiently by signing up for free. Sign up free

Chemical-Lead-ASTM-B29 — Lead Alloy

Category
Lead Alloy
Material Id
Chemical Lead ASTM B29
Brinell Hardness (HB)
5
Cte per K (1/K)
0.000029
Density Kg M3 (kg/m3)
11,340
Elastic Modulus MPa (MPa)
16,000
Elongation Percent (%)
45
Grade
Copper-Bearing Lead
Heat Treatment
As-cast/wrought
Melting Point C (°C)
327
Name
Chemical Lead (Pb-0.04–0.08Cu)
Specific Heat J kgK (J/(kg·K))
128
Standard
ASTM B29
Tensile Strength MPa (MPa)
20
Thermal Conductivity W mK (W/(m·K))
35
Yield Strength MPa (MPa)
8

Source: ASTM B29