Stellite-6B-Wrought-Annealed — Cobalt Alloy

Category
Cobalt Alloy
Material Id
Stellite 6B Wrought Annealed
Brinell Hardness (HB)
36
Cte per K (1/K)
0.000016
Density Kg M3 (kg/m3)
8,390
Elastic Modulus MPa (MPa)
212,000
Elongation Percent (%)
11
Grade
R30016
Heat Treatment
Solution Heat-Treated
Melting Point C (°C)
1,310
Name
Stellite 6B (Co-28Cr-4W-1C) Wrought
Specific Heat J kgK (J/(kg·K))
423
Standard
Kennametal Stellite / High Temp Metals (Stellite 6B Technical Data)
Tensile Strength MPa (MPa)
985
Thermal Conductivity W mK (W/(m·K))
14.8
Yield Strength MPa (MPa)
610

Source: Kennametal Stellite / High Temp Metals (Stellite 6B Technical Data)

cobalt_alloy — material id Stellite_6B_Wrought_Annealed · name Stellite 6B (Co-28Cr-4W-1C) wrought · standard Kennametal Stellite / High Temp Metals (Stellite 6B Technical Data) · density kg m3 8390 kg/m3 · heat treatment solution heat-treated | Metal Alloy Properties | Engineering Database