DIN-Gts-40 — Cast Iron

Category
Cast Iron
Material Id
DIN Gts - 40
Cte per K (1/K)
0.000011
Density Kg M3 (kg/m3)
7,160
Elastic Modulus MPa (MPa)
160,000
Elongation Percent (%)
4
Melting Point C (°C)
1,175
Name
DIN Gts - 40
Poisson Ratio (dimensionless)
0.27
Shear Modulus MPa (MPa)
64,000
Specific Heat J kgK (J/(kg·K))
460
Standard
DIN
Tensile Strength MPa (MPa)
400
Thermal Conductivity W mK (W/(m·K))
46
Vickers Hardness (HV)
220
Yield Strength MPa (MPa)
180

Source: DIN

cast_iron — material id DIN_GTS_-_40 · name DIN GTS - 40 · yield strength MPa 180 MPa · tensile strength MPa 400 MPa | Metal Alloy Properties | Engineering Database