Csn-422435 — Cast Iron
- Category
- Cast Iron
- Material Id
- Csn 422435
- Cte per K (1/K)
- 0.000011
- Density Kg M3 (kg/m3)
- 7,160
- Elastic Modulus MPa (MPa)
- 115,000
- Melting Point C (°C)
- 1,175
- Name
- Csn 422435
- Poisson Ratio (dimensionless)
- 0.25
- Shear Modulus MPa (MPa)
- 46,000
- Specific Heat J kgK (J/(kg·K))
- 460
- Standard
- Csn
- Tensile Strength MPa (MPa)
- 350
- Thermal Conductivity W mK (W/(m·K))
- 46
- Vickers Hardness (HV)
- 260
- Yield Strength MPa (MPa)
- 350
Source: CSN