Metal Alloy Properties: aluminum alloy
Al-Li 8090 T8771 45deg 80K to Al-Li 8090 T8771 L 80K
Metal and alloy mechanical properties — tensile/yield strength, elastic modulus, density, hardness for steels, aluminum alloys, copper alloys, titanium, nickel alloys, cast iron, and more
| category | material id | density kg m3 (kg/m3) | elongation percent (%) | grade | heat treatment | name | property basis | reduction percent (%) | specific heat J kgK (J/(kg·K)) | standard | tensile strength MPa (MPa) | test direction | test temperature C (C) | thermal conductivity W mK (W/(m·K)) | yield strength MPa (MPa) |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| aluminum alloy | Al-Li 8090 T8771 45deg 80K | 2,600 | 13.966667 | 8090-T8771 | T8771 | Al-Li 8090-T8771 45 Degree | Typical | 13.666667 | — | NISTIR 3971 | 559 | 45 Degree | -193.15 | 29.9 | 388.666667 |
| aluminum alloy | Al-Li 8090 T8771 L | 2,600 | 5.871429 | 8090-T8771 | T8771 | Al-Li 8090-T8771 Longitudinal | Typical | 7.1 | 969 | NISTIR 3971 | 508.571429 | Longitudinal | — | 78.7 | 450.142857 |
| aluminum alloy | Al-Li 8090 T8771 L 200K | 2,600 | 6.766667 | 8090-T8771 | T8771 | Al-Li 8090-T8771 Longitudinal | Typical | 11.366667 | 830 | NISTIR 3971 | 524.666667 | Longitudinal | -73.15 | 59.2 | 458.333333 |
| aluminum alloy | Al-Li 8090 T8771 L 20K | 2,600 | 13.7 | 8090-T8771 | T8771 | Al-Li 8090-T8771 Longitudinal | Typical | 12.9 | — | NISTIR 3971 | 798.5 | Longitudinal | -253.15 | 11.6 | 570.5 |
| aluminum alloy | Al-Li 8090 T8771 L 365K | 2,600 | 7.366667 | 8090-T8771 | T8771 | Al-Li 8090-T8771 Longitudinal | Typical | 12.133333 | 1,038 | NISTIR 3971 | 503 | Longitudinal | 91.85 | — | 460 |
| aluminum alloy | Al-Li 8090 T8771 L 480K | 2,600 | 18.4 | 8090-T8771 | T8771 | Al-Li 8090-T8771 Longitudinal | Typical | 57.233333 | — | NISTIR 3971 | 340.666667 | Longitudinal | 206.85 | — | 336.333333 |
| aluminum alloy | Al-Li 8090 T8771 L 535K | 2,600 | 19.25 | 8090-T8771 | T8771 | Al-Li 8090-T8771 Longitudinal | Typical | 82.3 | — | NISTIR 3971 | 186.5 | Longitudinal | 261.85 | — | — |
| aluminum alloy | Al-Li 8090 T8771 L 5K | 2,600 | 9.64 | 8090-T8771 | T8771 | Al-Li 8090-T8771 Longitudinal | Typical | 15.5 | — | NISTIR 3971 | 714.4 | Longitudinal | -268.15 | — | 573.5 |
| aluminum alloy | Al-Li 8090 T8771 L 75K | 2,600 | 11.4 | 8090-T8771 | T8771 | Al-Li 8090-T8771 Longitudinal | Typical | 11 | — | NISTIR 3971 | 699 | Longitudinal | -198.15 | 29.9 | 542 |
| aluminum alloy | Al-Li 8090 T8771 L 80K | 2,600 | 8.233333 | 8090-T8771 | T8771 | Al-Li 8090-T8771 Longitudinal | Typical | 7.866667 | — | NISTIR 3971 | 626 | Longitudinal | -193.15 | 29.9 | 507.333333 |
What else is in Engineering Database
Iron Engine ↗Engineering AI at ironengine.ai
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators