Ciir — Iir

Elastomer
Iir
Grade Or Variant
Ciir
Acid Resistance
Excellent
ASTM Designation
AA, Ba (ASTM D2000)
Chemical Resistance Notes
Same Chemical Resistance As IIR; Improved Compression set, heat, ozone, and Flex Fatigue vs Standard IIR; Can Be Co-Cured with EPDM, NR, Sbr
Common Name
Chlorobutyl Rubber
Compression Set Pct (%)
25-50
Compression Set Temp C
100
Compression Set Time Hr
22
Cure System
sulfur, resin, Zinc oxide, Or Peroxide
Density G CM3 (g/cm3)
1.15-1.35
Elongation at Break Pct (%)
400-800
Fuel Resistance
Poor
Gas Permeability
Very Low
Glass Transition Temp C (C)
-70
Hardness Range Shore a
35-95
Max Continuous Temp C (C)
105
Max Peak Temp C (C)
120
Max Service Temp C (C)
105
Min Service Temp C (C)
-55
Oil Resistance
Poor
Ozone Resistance
Excellent
Steam Resistance
Good
Tensile Strength Mpa (MPa)
7-17
IIR — grade or variant CIIR · chemical resistance notes Same chemical resistance as IIR; improved compression set, heat, ozone, and… · common name Chlorobutyl Rubber · max continuous temp C 105 C · max service temp C 105 C | Elastomer Service Properties | Engineering Database