Home/Reference Data/Concrete Admixtures

Concrete Admixtures

Concrete chemical admixture reference data — ASTM C494 Types A/B/C/D/E/F/G/S, ASTM C260 air-entraining, calcium nitrite corrosion inhibitors, VMA, SRA, and lithium nitrate ASR mitigation. Parameters include dosage range (mL/100 kg cement), water reduction (%), initial/final set time change (min), compressive strength effect at 1/7/28 days (%), slump increase (mm), air content change (%), and compatibility notes.

Civil Engineering10 sections21 sample rowsKey: admixture_type

Attributes

astm_standard
common_name
dosage_min_mL_per_100kgmL/100kg-cement
dosage_typical_mL_per_100kgmL/100kg-cement
dosage_max_mL_per_100kgmL/100kg-cement
water_reduction_min_pct%
water_reduction_typical_pct%
water_reduction_max_pct%
set_time_change_initial_minminutes
set_time_change_final_minminutes
strength_1d_pct_change%
strength_7d_pct_change%
strength_28d_pct_change%
slump_increase_mmmm
air_content_change_pct%
compatibility_notes

Browse data

Search the full concrete admixtures dataset with natural language or structured queries.

Search this table