Explore the Engineering Database more efficiently by signing up for free. Sign up free
70-Inconel-706-Bar-Forging-Ht-2.500-LT2.500-4.000-S-T6-3-4-0B-C7 — Inconel 706 Bar Forging Ht 2.500-LT2.500
- Material Id
- Inconel 706 Bar Forging Ht 2.500-LT2.500 4.000 S T6 3 4 0B C7
- Temp F
- 70
- E Msi (Msi)
- 30.4
- Ec Msi (Msi)
- 30.4
- Fbru Ksi (ksi)
- 256
- Fbru Ksi 2 (ksi)
- 325
- Fbry Ksi (ksi)
- 181
- Fbry Ksi 2 (ksi)
- 218
- Fcy Ksi (ksi)
- 136
- Fsu Ksi (ksi)
- 103
- Ftu Ksi (ksi)
- 165
- Fty Ksi (ksi)
- 130
- G Msi (Msi)
- 11
- Ra Pct (%)
- 15
- Basis
- S
- Condition
- Heat Treated per Indicated Specification
- Density Lb IN3 (lb/in^3)
- 0.292
- Elongation Pct (%)
- 12
- Form
- Bar and Forging
- Poisson Ratio
- 0.38
- Specification
- AMS AMS 5702 and AMS 5701 5606 AMS 5703
- Thickness Range
- 2.500-<2.500 4.000