Explore the Engineering Database more efficiently by signing up for free. Sign up free
Home/Reference Data/Aerospace Materials/Inconel 706 Bar Forging Ht 2.500-LT2.500/70-INCONEL-706-BAR-FORGING-HT-2.500-LT2.500-4.000-S-T6-3-4-0b-C4

70-Inconel-706-Bar-Forging-Ht-2.500-LT2.500-4.000-S-T6-3-4-0B-C4 — Inconel 706 Bar Forging Ht 2.500-LT2.500

Material Id
Inconel 706 Bar Forging Ht 2.500-LT2.500 4.000 S T6 3 4 0B C4
Temp F
70
E Msi (Msi)
30.4
Ec Msi (Msi)
30.4
Fbru Ksi (ksi)
263
Fbru Ksi 2 (ksi)
334
Fbry Ksi (ksi)
195
Fbry Ksi 2 (ksi)
234
Fcy Ksi (ksi)
146
Fsu Ksi (ksi)
106
Ftu Ksi (ksi)
170
Fty Ksi (ksi)
140
G Msi (Msi)
11
Ra Pct (%)
15
Basis
S
Condition
Heat Treated per Indicated Specification
Density Lb IN3 (lb/in^3)
0.292
Elongation Pct (%)
12
Form
Bar and Forging
Poisson Ratio
0.38
Specification
AMS AMS 5702 and AMS 5701 5606 AMS 5703
Thickness Range
2.500-<2.500 4.000
INCONEL 706 BAR FORGING HT 2.500-LT2.500 — temp f 70 · material id INCONEL_706_BAR_FORGING_HT_2.500-LT2.500_4.000_S_T6_3_4_0b_C4 · Fbry ksi 195 ksi · Fbry ksi 2 234 ksi · Fcy ksi 146 ksi | Aerospace Materials | Engineering Database