Explore the Engineering Database more efficiently by signing up for free. Sign up free

70-7075-Forging-T652-LE2.000-S — 7075 Forging T652

Material Id
7075 Forging T652 LE2.000 S
Temp F
70
E Msi (Msi)
10
Ec Msi (Msi)
10.4
Fcy Ksi (ksi)
63
Fcy Ksi Lt (ksi)
61
Fsu Ksi (ksi)
44
Ftu Ksi (ksi)
74
Ftu Ksi Lt (ksi)
73
Fty Ksi (ksi)
63
Fty Ksi Lt (ksi)
61
G Msi (Msi)
3.8
Basis
S
Condition
T652
Density Lb IN3 (lb/in^3)
0.101
Elongation Pct (%)
9
Elongation Pct Lt (%)
4
Form
Hand Forging
Poisson Ratio
0.33
Specification
AMS-a-22771 and AMS-Qq-a-367
Thickness Range
<=2.000