Home/Reference Data/Aerospace Materials/7075 Forging T652/70-7075-FORGING-T652-5.001-6.000-S-T3-7-6-0f1-C9

70-7075-Forging-T652-5.001-6.000-S-T3-7-6-0F1-C9 — 7075 Forging T652

Material Id
7075 Forging T652 5.001-6.000 S T3 7 6 0F1 C9
Temp F
70
E Msi (Msi)
10
Ec Msi (Msi)
10.4
Fsu Ksi (ksi)
41
Ftu Ksi (ksi)
69
Ftu Ksi Lt (ksi)
68
Ftu Ksi St (ksi)
66
Fty Ksi (ksi)
58
Fty Ksi Lt (ksi)
56
Fty Ksi St (ksi)
55
G Msi (Msi)
3.8
Basis
S
Condition
T652
Density Lb IN3 (lb/in^3)
0.101
Elongation Pct (%)
7
Elongation Pct Lt (%)
3
Elongation Pct St (%)
1
Form
Hand Forging
Poisson Ratio
0.33
Specification
AMS-a-22771 and AMS-Qq-a-367
Thickness Range
5.001-6.000